Product Description
At a Glance
2507 is where duplex goes when 2205 is not enough. At 25% chromium, 7% nickel, 4% molybdenum and 0.27% nitrogen it reaches PREN ≈ 42, which puts its critical pitting temperature in seawater some 20–30 °C above 2205. Yield strength rises to 550 MPa. It is specified for hot seawater, high chloride concentrations and high pressure.
What 'Super' Actually Buys You
The step from 2205 to 2507 is not a small one. Chromium goes from 22% to 25%, molybdenum from 3.2% to 4%, and nitrogen from 0.17% to 0.27%. Because nitrogen counts sixteen times in the pitting calculation, that last change matters most: PREN moves from about 35 to about 42. In practice the critical pitting temperature in seawater rises by roughly 20–30 °C, which is the difference between 2205 working and 2205 pitting. Yield strength goes from 450 to 550 MPa at the same time. What it costs you is formability — elongation drops to 15% — and a narrower welding window.
Where 2507 Coil Gets Used
Grade Cross-Reference
Chemical Composition (ASTM A240, % by weight)
Mechanical Properties (annealed, room temperature)
Surface Finish Guide
Size Range & Weight
Figures are calculated from the alloy density and are for estimating only — actual weight follows the mill's measured thickness.
Processing Services
Where 2507 Is the Wrong Choice
Above roughly 300 °C, 2507 precipitates sigma phase faster than 2205 because of its higher chromium and molybdenum. The 300 °C ceiling is firm.
At 15% elongation, formability is very limited. Complex bending and any drawing will crack. Buy formed parts rather than trying to form thin super duplex coil.
The welding window is narrow: interpass temperature typically held to 100 °C with controlled heat input. It is not a job for a shop without duplex experience.
For indoor or mild service it is expensive over-specification — several times the price of 316L.
Ordering & Delivery
FAQ
2507 against 2205?
PREN about 42 against 35, and yield 550 against 450. Choose 2507 for hot seawater, high chloride or high pressure; 2205 is enough for everything else and costs less.
Is it magnetic?
Yes — like all duplex grades, the ferrite phase makes it magnetic.
Can it be welded?
Yes, but it demands discipline. ER2594 filler, controlled heat input, interpass temperature held down. Confirm your fabricator has duplex procedure qualification before you commit.
15% elongation — is that going to be a problem?
For bending and rolling, yes. It limits what you can form. Send us the forming sequence before ordering and we will tell you whether coil is the right form.
Why the 300 °C cap?
Sigma phase and other intermetallics precipitate above roughly 300 °C and the material embrittles. 2507 is more sensitive than 2205, not less.
Is S32760 the same material?
Close, not identical. Zeron 100 adds tungsten and copper. It is often accepted as fit for purpose, but check your design code before substituting.
Tell Us Four Things — We'll Come Back With a Price
2507 enquiries — chloride level and peak temperature decide it. Send both and we will tell you honestly whether 2205 would do the job.
01 Grade — 2507
02 Thickness × width, and coil or slit strip
03 Finish — 2B or No.1
04 Quantity, chloride concentration and service temperature
WhatsApp: +86 13516180717
Email: jiutai@hanyang-steel.com
We come back with a written quote within 12 hours, Shanghai time — price, lead time, packing and loading port on one page. No forms, no waiting on a callback.
Product Show

Partner
Packaging and Shipping

Get Your Free Quote Now!
Related Products
Thank you very much for writing to us. Please leave your message and contact information, we will reply to you within 24 hours.