ASTM A240 310S Stainless Steel Coil & Strip — 25Cr-20Ni for Continuous High-Temperature Service
310S is the grade you move to when 304 and 321 stop coping. With 25% chromium and 20% nickel it holds a protective oxide scale in air at temperatures where lower alloys spall and scale away. The 'S' means low carbon, which keeps it weldable and ductile.
Contact Us

‹

ASTM A240 310S Stainless Steel Coil & Strip — 25Cr-20Ni for Continuous High-Temperature Service

›

‹

›

Product Description

 At a Glance

310S is the grade you move to when 304 and 321 stop coping. With 25% chromium and 20% nickel it holds a protective oxide scale in air at temperatures where lower alloys spall and scale away. The 'S' means low carbon, which keeps it weldable and ductile.

Item

Range

Grade

310S (310 available on request)

Standard

ASTM A240 / A480 · UNS S31008 · EN 10088-2 · JIS G4305

Thickness

0.3 – 3.0 mm (to 6.0 mm on request)

Width

Coil 1000 / 1219 / 1500 mm · Strip slit from 10 mm up

Coil ID

508 mm / 610 mm

Coil weight

2 – 8 MT per coil, packed to container limit

Surface finish

No.1 · 2B · BA · No.4

Oxidation resistance in air

Up to about 1150 °C

Certificate

EN 10204 3.1 mill test certificate, heat number traceable

 Why 25 Chromium and 20 Nickel

Two things have to happen at once in a furnace part. Chromium forms an oxide scale that protects the metal underneath, and it takes roughly 25% chromium to keep that scale stable at 1100 °C and above. Nickel keeps the structure austenitic so the part does not embrittle or crack as it cycles through temperature. 304 carries 18% chromium and 8% nickel — enough for a kitchen sink, not enough for a furnace muffle. That is the whole reason 310S exists.

 Where 310S Coil Gets Used

Application

Why this grade

Furnace linings, muffles, annealing covers

Holds its oxide scale through continuous high-temperature cycles

Kiln furniture, heat treatment fixtures and baskets

Resists scaling where 304 or 321 would flake away

Radiant tubes and burner components

High chromium handles the hot face

Incineration and boiler hot sections

Oxidation and thermal cycling together

Glass and ceramic industry fixtures

Stable at temperature, resists spalling

Petrochemical reformer and furnace internals

Standard high-temperature austenitic choice

 Grade Cross-Reference

System

Designation

UNS

S31008

EN / DIN

1.4845 · X8CrNi25-21

JIS

SUS310S

GB

06Cr25Ni20 (old 0Cr25Ni20)

Related

310 — higher carbon, specified for creep strength

Not the same as

321 — 321 is stabilised for the 425–815 °C band, not for furnace temperatures

 Chemical Composition (ASTM A240, % by weight)

Element

Range

Carbon (C)

0.08 max

Manganese (Mn)

2.00 max

Phosphorus (P)

0.045 max

Sulfur (S)

0.030 max

Silicon (Si)

1.50 max — supports oxidation resistance

Chromium (Cr)

24.0 – 26.0

Nickel (Ni)

19.0 – 22.0

Molybdenum (Mo)

0.75 max

Nitrogen (N)

0.10 max

 Mechanical Properties (annealed, room temperature)

Property

Value

Yield strength, 0.2% offset

205 MPa min (30 ksi)

Tensile strength

515 MPa min (75 ksi)

Elongation in 50 mm

40% min

Hardness

217 HB max / 95 HRB max

Density

7.98 g/cm³

Magnetic in annealed condition

No (austenitic)

 Surface Finish Guide

Finish

What it looks like

Choose it when

2B

Smooth, matte grey — the mill default

General fabrication, further forming, welding

BA

Bright, near-mirror, reflective

Visible trim, appliances, where appearance sells

No.4

Brushed directional grain

Architectural panels, elevator cabs, kitchen equipment

HL

Continuous long-grain polish

Wall cladding, column covers, large visible areas

No.1

Hot rolled, annealed and pickled, dull grey

Furnace and high-temperature work, no cosmetic requirement

 Size Range & Weight

Figures are calculated from the alloy density and are for estimating only — actual weight follows the mill's measured thickness.

Thickness

Approx. m² per tonne

Typical use

0.5 mm

251

Thin furnace linings, shims, flexible parts

0.8 mm

157

Light fixtures, ducting

1.0 mm

125

General furnace panels, baskets

1.5 mm

84

Muffles, annealing covers

2.0 mm

63

Kiln furniture, structural fixtures

3.0 mm

42

Heavy hot-section components

 Processing Services

Service

What we do

Charged?

Slitting

Coil slit to your width, typically ±0.1 mm

Charged, quoted per tonne

Cut to length

Decoiled, levelled and cut to sheet length

Charged, quoted per tonne

Edge conditioning

Deburred or rounded slit edge

Charged on request

Protective film

PE or PVC film applied to protect the surface

Charged, recommended for BA and No.4

Export packing

Eye-to-sky or eye-to-wall, steel strapped, seaworthy

Included

Mill certificate

EN 10204 3.1, heat number traceable

Included

 Where 310S Is the Wrong Choice

Long holds between roughly 550 and 850 °C can precipitate sigma phase and embrittle 310S. If your part sits in that band continuously, 321 is usually the better answer.

In reducing or sulphur-bearing atmospheres the chromium oxide scale does not protect. High-nickel alloys are the right call there — tell us the atmosphere.

For room-temperature corrosion jobs you are paying for 20% nickel you will never use. 304 or 316L costs far less.

 Ordering & Delivery

Item

Terms

MOQ

25 MT per size, or 1 × 20' GP container. Mixed sizes in one container are negotiable.

Lead time

7–15 days ex-stock · 25–35 days to mill order

Payment terms

100% T/T in advance for small orders; 30% T/T deposit with the balance by irrevocable L/C at sight for standard orders; terms for large orders are negotiable.

Price basis

EXW · FOB · CFR · CIF · DAP

Loading port

Based on the actual port of shipment

Packing

Eye-to-sky or eye-to-wall on wooden skids, steel strapped, waterproof paper + PE film, edge protectors, coils separated by spacers. Seaworthy export packing standard.

Documentation

EN 10204 3.1 mill test certificate, packing list, commercial invoice, certificate of origin, fumigation certificate where required

Third-party inspection

SGS / BV / TUV / Intertek arranged on request (buyer's cost unless agreed otherwise)

Sample

Small sample piece free of charge; courier cost on the buyer's account

 FAQ

What is the maximum service temperature?

Oxidation resistance in air runs to about 1150 °C. Load-bearing capacity falls away well before that, so the design temperature is usually lower — send us your code and we will confirm.

310 or 310S?

310 has higher carbon for creep strength at temperature. 310S is low carbon, which makes it weldable and more ductile. We ship 310S as standard.

Can it be welded?

Yes, readily, with matching 310 filler. No preheat is required and post-weld annealing is not normally needed.

Why does the price move so much?

20% nickel. The alloy price tracks the LME nickel price closely, so ask us for a validity window on any quotation.

Is 310S magnetic?

No, it is fully austenitic in the annealed condition.

Will it survive thermal cycling?

Yes — better than most grades. The high nickel content is what keeps it from embrittling through repeated heating and cooling.

 Tell Us Four Things — We'll Come Back With a Price

 310S enquiries — the atmosphere and peak temperature matter more than the thickness. Send both and we will confirm the grade.

  01  Grade — 310S or 310

  02  Thickness × width, and coil or slit strip

  03  Finish — No.1 for furnace work, 2B otherwise

  04  Quantity, maximum service temperature and atmosphere

 

 WhatsApp: +86 13516180717    

Email: jiutai@hanyang-steel.com

 We come back with a written quote within 12 hours, Shanghai time — price, lead time, packing and loading port on one page. No forms, no waiting on a callback.



Product Show

ASTM A240 310S Stainless Steel Coil & Strip — 25Cr-20Ni for Continuous High-Temperature Service

Partner

Packaging and Shipping

ASTM A240 310S Stainless Steel Coil & Strip — 25Cr-20Ni for Continuous High-Temperature Service

Get Your Free Quote Now!

Submit